Mechanical Properties Metric English Comments
Flexural Modulus 4.41 GPa

@Temperature 23.0 °C
640 ksi

@Temperature 73.4 °F
DAM; ASTM D790
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers