Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Flexural Modulus | 2.80 GPa @Temperature -40.0 °C |
406 ksi @Temperature -40.0 °F |
ASTM-D790 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Flexural Modulus | 2.80 GPa @Temperature 80.0 °C |
406 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 2.80 GPa @Temperature 80.0 °C |
406 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.5%); ASTM-D790 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D.. |
|||
Flexural Modulus | 2.80 GPa @Temperature 150 °C |
406 ksi @Temperature 302 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |