Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 28.2 GPa @Temperature 177 °C |
4090 ksi @Temperature 351 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement Laminate Physicals: 53% Fiber volume, 29% Resin content, 0.5% VoidsInformation provided by HexCel |