Mechanical Properties Metric English Comments
Flexural Modulus 2.90 GPa

@Temperature -40.0 °C
421 ksi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.90 GPa

@Temperature 23.0 °C
421 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.90 GPa

@Temperature 23.0 °C
421 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer
Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod..
Flexural Modulus 2.90 GPa

@Temperature 23.0 °C
421 ksi

@Temperature 73.4 °F
ASTM D790
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..
Flexural Modulus 2.90 GPa

@Temperature 80.0 °C
421 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..