Mechanical Properties Metric English Comments
Flexural Modulus 30.0 GPa

@Temperature 150 °C
4350 ksi

@Temperature 302 °F
ISO 178
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex..
Flexural Modulus 30.0 GPa

@Temperature 250 °C
4350 ksi

@Temperature 482 °F
ISO 178
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex..