Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.241 GPa @Temperature -40.0 °C |
470.1 ksi @Temperature -40.0 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |