Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.99 GPa @Temperature 93.0 °C |
579 ksi @Temperature 199 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |