Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.00 GPa @Temperature 23.0 °C |
870 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
Flexural Modulus | 6.00 GPa @Temperature 23.0 °C |
870 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
Flexural Modulus | 6.00 GPa @Temperature 23.0 °C |
870 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.6%); ASTM-D790 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |