Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.24 GPa @Temperature 23.0 °C |
760 ksi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |