Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.30 GPa @Temperature 23.0 °C |
769 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 5.30 GPa @Temperature 23.0 °C |
769 ksi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 5.30 GPa @Temperature 177 °C |
769 ksi @Temperature 351 °F |
Autoclave Cured; [90°]16; Wet condition |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |
|||
Flexural Modulus | 5.30 GPa @Temperature 177 °C |
769 ksi @Temperature 351 °F |
T300 (6K); [90°]16; Wet Condition |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |