Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.07 GPa @Temperature 65.6 °C |
1170 ksi @Temperature 150 °F |
|
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive .. |