Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.66 GPa @Temperature -40.0 °C |
1400 ksi @Temperature -40.0 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |