Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.21 GPa @Thickness 1.57 mm |
900 ksi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Flexural Modulus | 6.21 GPa @Thickness 2.50 mm, Temperature 150 °C |
900 ksi @Thickness 0.0984 in, Temperature 302 °F |
Secant; ISO 178 |
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo.. |