Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.34 GPa

@Temperature 121 °C
920 ksi

@Temperature 250 °F
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization
Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive ..