Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.320 J/cm

@Thickness 12.7 mm
0.600 ft-lb/in

@Thickness 0.500 in
LW, E-48/50
Industrial Laminates/Norplex ES-1 Engraving Stock
Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620”, 0.125”, and 0.500”
Izod Impact, Unnotched 0.320 J/cm

@Thickness 12.7 mm
0.600 ft-lb/in

@Thickness 0.500 in
LW, E-48/50
Industrial Laminates/Norplex ES-2 Engraving Stock
Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies.
Izod Impact, Unnotched 0.320 J/cm

@Thickness 12.7 mm
0.600 ft-lb/in

@Thickness 0.500 in
LW, E-48/50
Industrial Laminates/Norplex ES-3 Engraving Stock
Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin.
Izod Impact, Unnotched 0.320 J/cm

@Thickness 12.7 mm
0.600 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP611 Paper Base Laminate
Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a..
Izod Impact, Unnotched 0.320 J/cm

@Thickness 12.7 mm
0.600 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP613 Paper Base Laminate
Description: NP613 is constructed from electrical grade of kraft paper and a specially modified epoxy resin system. It is designed to be used in tap changers, coil support plates and terminal panels..
Izod Impact, Unnotched 0.320 J/cm

@Thickness 12.7 mm
0.600 ft-lb/in

@Thickness 0.500 in
CW, E-48/50
Industrial Laminates/Norplex NP631 Paper Base Laminate
Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500"
Izod Impact, Unnotched 0.320 J/cm

@Thickness 12.7 mm
0.600 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...