Polymer Property : Izod Impact, Unnotched = 0.392 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.392 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
0.735 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical TR300 MABS, Flame Retardant, Transparency
Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch..
Izod Impact, Unnotched 0.392 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
0.735 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical TR300 MABS, Flame Retardant, Transparency
Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch..
Izod Impact, Unnotched 0.392 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
0.735 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf..
Izod Impact, Unnotched 0.392 J/cm

@Thickness 6.40 mm,
Temperature -20.0 °C
0.735 ft-lb/in

@Thickness 0.252 in,
Temperature -4.00 °F
ASTM D256
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 0.392 J/cm

@Thickness 3.20 mm,
Temperature -20.0 °C
0.735 ft-lb/in

@Thickness 0.126 in,
Temperature -4.00 °F
ASTM D256
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical