Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.315 J/cm

@Thickness 12.7 mm
0.590 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP615 Paper Base Laminate
Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated ..