Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.534 J/cm @Thickness 12.7 mm |
1.00 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP310U Cotton Fabric Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0... |