Mechanical Properties Metric English Comments
Izod Impact, Unnotched 11.8 J/cm

@Temperature 23.0 °C
22.1 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.