Mechanical Properties Metric English Comments
Izod Impact, Unnotched 6.41 J/cm

@Thickness 12.7 mm
12.0 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP130 Glass Fabric
Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic..
Izod Impact, Unnotched 6.41 J/cm

@Thickness 12.7 mm
12.0 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
Izod Impact, Unnotched 6.41 J/cm

@Thickness 12.7 mm
12.0 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP511 Glass Fabric
Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat..
Izod Impact, Unnotched 6.40 J/cm

@Temperature -40.0 °C
12.0 ft-lb/in

@Temperature -40.0 °F
ASTM D4812
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers