Polymer Property : Izod Impact, Unnotched = 2.60 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.39 J/cm

@Thickness 12.7 mm
2.60 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP321 Cotton Fabric  (discontinued **)
Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f..