Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.67 J/cm

@Thickness 8.00 mm
5.00 ft-lb/in

@Thickness 0.315 in
LW, E-48/50
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric
Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined..
Izod Impact, Unnotched 2.67 J/cm

@Temperature -30.0 °C
5.00 ft-lb/in

@Temperature -22.0 °F
ASTM D 4812
SABIC Innovative Plastics Noryl PX4058 PPE+PS
PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 2.67 J/cm

@Temperature -30.0 °C
5.00 ft-lb/in

@Temperature -22.0 °F
ASTM D 4812
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific)
PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region.