Mechanical Properties Metric English Comments
Izod Impact, Unnotched 12.8 J/cm

@Thickness 12.7 mm
24.0 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP193P Synthetic Fabric
Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp..
Izod Impact, Unnotched 12.8 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
24.0 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Izod Impact, Unnotched 12.8 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
24.0 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..