Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.00 J/cm

@Thickness 4.00 mm,
Temperature -20.0 °C
3.75 ft-lb/in

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PPE 1462  (discontinued **)