Polymer Property : Izod Impact, Unnotched = 32.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 17.1 J/cm

@Thickness 12.7 mm
32.0 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP193M Synthetic Fabric Base Grade
Description: 17 oz. aramide and “soft glass” fibers are combined to make a fabric that is stronger than pure aramide and less abrasive than glass fabrics. This material is impregnated with..