Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.99 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
5.99 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |