Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 6.00 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
11.2 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PP 1380
PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR..
Izod Impact, Unnotched 6.00 J/cm

@Temperature -30.0 °C
11.2 ft-lb/in

@Temperature -22.0 °F
ASTM D 4812
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific)
XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r..