Polymer Property : Flexural Modulus = 0.0000193 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0000193 - 29.0 GPa
0.00280 - 4200 ksi
Average value: 16.1 GPa Grade Count:25
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Flexural Modulus 0.0000193 GPa
0.00280 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 CF30 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf..