Mechanical Properties Metric English Comments
Flexural Modulus 0.006827 GPa
0.9902 ksi
ASTM D790
Sekisui PIOCELAN SP-50D Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..