Polymer Property : Flexural Modulus = 0.0100 GPa
Polymer Property :
Flexural Modulus =
0.0100 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
0.00800
-
0.0100
GPa
1.16
-
1.45
ksi
ISO 178
PolyOne Bergadurâ„¢ PB400 G30 UF UV Polybutylene Terephthalate (PBT)
Information provided by PolyOne