Mechanical Properties Metric English Comments
Flexural Modulus 0.01025 - 0.01075 GPa
1.487 - 1.559 ksi
FiberNide Nickel Aluminide Foam Atomic 10% Aluminum
Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f..