Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0172 GPa | 2.50 ksi | 2% Secant, in accordance with ASTM D638; ASTM D790 |
M. Holland Company MAGMA® LM372-A LLDPE