Polymer Property : Flexural Modulus = 0.0180 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0180 GPa

@Temperature 49.0 °C
2.61 ksi

@Temperature 120 °F
ASTM D790
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0180 GPa
2.61 ksi
ASTM D638
Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a poly..