Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0310 GPa | 4.50 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Flexural Modulus | 0.0310 GPa @Temperature 49.0 °C |
4.50 ksi @Temperature 120 °F |
ASTM D790 |
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.0310 GPa | 4.50 ksi | ASTM D790 |
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Flexural Modulus | 0.0310 GPa | 4.50 ksi | ASTM D790 |
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane Type: Estane® ALR PC95A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
Flexural Modulus | 0.0310 GPa | 4.50 ksi | 1% secant; ASTM D790 |
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Flexural Modulus | 0.0310 GPa | 4.50 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A |
Dow FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |