Mechanical Properties Metric English Comments
Flexural Modulus 0.0420 GPa
6.09 ksi
ISO 178
Huntsman AVALON® 90 AB Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
Flexural Modulus 0.0420 GPa
6.09 ksi
ISO 178
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling ..