Mechanical Properties Metric English Comments
Flexural Modulus 0.0454 GPa
6.58 ksi
1% secant; ASTM D790
ExxonMobil Escorene® LD 722.MV Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 722.MV is a high vinyl acetate copolymer resin for specialty extrusion and compounding application. Articles made from LD 722.MV are soft and have excellent low temperature toughne..