Polymer Property : Flexural Modulus = 0.0580 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0580 GPa
8.41 ksi
ISO 178
DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Light ProtectionInformation provided by DuPont Performance Polymers