Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0637 GPa | 9.25 ksi | ASTM D790 |
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided .. |