Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0750 GPa | 10.9 ksi | Conditioned 15 days at 23°C - 50% RH; ISO178 |
Arkema Group Pebax® Rnew 40R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 40R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Flexural Modulus | 0.0750 GPa | 10.9 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR5020 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |