Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0869 GPa | 12.6 ksi | ASTM D790 |
Ecomass® 4703ZC57 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |