Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.113 GPa | 16.4 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 9002 GREY/BROWN Ash is 15%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.113 GPa | 16.4 ksi | ISO 178 |
Gromax 1140LH TPE Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject.. |
|||
Flexural Modulus | 0.113 GPa | 16.4 ksi | ASTM D790 |
Ecomass® 4703ZD88 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym.. |