Polymer Property : Flexural Modulus = 0.157 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.157 GPa
22.8 ksi
ASTM D790
DuPont 20 Series DPE 20 Specialty Polyethylene Resin
DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex..