Mechanical Properties Metric English Comments
Flexural Modulus 0.184 GPa
26.7 ksi
ISO 178
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi..