Mechanical Properties Metric English Comments
Flexural Modulus 0.197 GPa

@Temperature -20.0 °C
28.6 ksi

@Temperature -4.00 °F
ASTM D790
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..