Polymer Property : Flexural Modulus = 0.2345 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.2345 GPa
34.01 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Flex® TPO D 4508 D 4508
This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase.