Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.248 GPa | 36.0 ksi | 1% Secant; ASTM D790 |
M. Holland Company LD500 LDPE
(discontinued **) Features: High Clarity, High Flow, Narrow Molecular Wt. Dist., Good Processability, Warp ResistantUses: Drink LidsApprovals: FDA 21 CFR 177.1520(c) 2.2 and ASTM D 1248, I, Class A, Cat. 1Processing .. |
|||
Flexural Modulus | 0.248 GPa | 36.0 ksi | |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |