Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00207 GPa | 0.300 ksi | ASTM D790 |
Teknor Apex TEKRON® 4000-25 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flexural Modulus | 0.00207 - 2.26 GPa | 0.300 - 327 ksi | Average value: 0.274 GPa Grade Count:120 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |