Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.338 - 0.400 GPa | 49.0 - 58.0 ksi | ASTM D790 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Flexural Modulus | 0.338 GPa | 49.0 ksi | ASTM D790(B) |
DuPont Surlyn® 9945 Thermoplastic Ionomer Resin Surlyn® 9945 provides high flow properties and consistent, easy processing behavior in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the i.. |