Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.454 GPa | 65.8 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 6407 Injection Molding Resin
(discontinued **) LL 6100 is a narrow molecular weight butene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal wa.. |