Polymer Property : Flexural Modulus = 0.620 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.580 - 0.620 GPa
84.1 - 89.9 ksi
ASTM D790
Zeus FEP Tubing
FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua..